Polymer Property : CTE, linear, Transverse to Flow = 49.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® FR30U ABS
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific)
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® HMG47MD ABS
General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47 ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47F ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47F ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant.
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47N ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti..
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MG47N ABS (Asia Pacific)
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti..
CTE, linear, Transverse to Flow 88.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycolac® MGABS02 ABS
General purpose ABS. Excellent flow/impact.
CTE, linear, Transverse to Flow 88.2 µm/m-°C
49.0 µin/in-°F
Diameter
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..