Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific)
Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 88.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL REN501 PPE+PS
Noryl REN501 resin is an unfilled Post Industrial Recycle (PIR) based injection moldable modified polyphenylene ether blend comprising up to 40% PIR content. Available in black only.
CTE, linear, Transverse to Flow 88.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
48.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL SE1X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications.
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
48.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KFI16 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KFI16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Silicone.
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66
LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant.
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
48.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RX05050 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RX05050 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT
LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant.
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS
LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive.
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
48.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON ZEF061XC PPO (Europe-Africa-Middle East)
LNP* STATKON* ZEF061XC is a compound based on Polyphenyleneoxide resin containing Glass Fiber, Milled Carbon Fiber and Flame Retardant. Added Features include: Electrically Conductive
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
48.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP KB008 Acetal Copolymer
LNP THERMOCOMP* KB008 is a compound based on Acetal Copolymer resin containing 40% Glass Bead.
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT
LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers.
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
48.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP
LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
48.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/2
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
CTE, linear, Transverse to Flow 88.0 µm/m-°C
48.9 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm..
CTE, linear, Transverse to Flow 88.0 - 88.0 µm/m-°C

@Temperature 60.0 - 138 °C
48.9 - 48.9 µin/in-°F

@Temperature 140 - 280 °F
Average value: 88.0 µm/m-°C Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature 20.0 °C
48.9 µin/in-°F

@Temperature 68.0 °F
TMA; ASTM E831
LNP Thermotuf® QF-1006 HI Polyamide 6/10 Copolymer, Glass Fiber Reinforcement  (discontinued **)
Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ..