Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex DS0026 PC (Europe-Africa-Middle East) LNP* Faradex* DS0026 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features include: EMI/RFI Shielding, Flame Retardant, Non-Brominated & Non-C.. |
|||
CTE, linear, Transverse to Flow | 65.0 - 180 µm/m-°C | 36.1 - 100 µin/in-°F | Average value: 104 µm/m-°C Grade Count:17 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11 LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon NX03602 PC+ABS (Asia Pacific) LNP* STAT-KON* NX03602 is a compound based on PC+ABS Blend resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supplied by.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11 LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 20.0 °C |
36.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Multilon DN-3520F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 20 % filler. Improved stiffness and high flowability realizes a thin w.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PF00CS PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00CS is a compound based on PA6 resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Apec® 1697 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Apec® 1797 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2665 MAS071 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 2667 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection moldi.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 6267 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Formerly Makrolon DP1-1872MVR (300 °C/1.2 kg) 19 cm3/10 minFlame retardantUL 94V-0/1.5 mmLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 3.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 6457 Polycarbonate, Flame Retardant Grade MVR (300 °C/1.2 kg) 12.5 cm3/10 minUL 94V-0/3.0 mmUV stabilizedeasy releaseinjection moldingavailable in transparent, translucent and opaque colorsPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 6717 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-05-9Global gradeFormerly Makrolon DP1-1853MVR (300 °C/1.2 kg) 3.0 cm3/10 minFlame retardantUL 94V-0/2.0 mmHigh viscosityBranchedUV stabilizedEasy releaseInjection molding - Me.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® AG2677 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transparent colors on.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® AL2447 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® FS 2000 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Low viscosityAs of 1 S.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT XE 3996 PA*-GF30 Product description: Grivory XE 3996 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO-Polymer designatio.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
36.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makrolon® ET3227 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® LQ2687 Polycarbonate ISO 7391-PC,MLR,(,,)-18-9MVR (300 °C/1.2 kg) 12.5 cm3/10 minOptical lensMedium viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear t.. |
|||
CTE, linear, Transverse to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | ISO 11359-1/-2 |
Covestro Makrolon® Rx1452 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |