Polymer Property : CTE, linear, Transverse to Flow = 35.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
Average below Tg; ISO 11359
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
Average below Tg; ISO 11359
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
19.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS.
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber
PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic..
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
19.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP EFB26ER PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EFB26ER is a compound based on Polyetherimide containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Mold Release.
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Teijin Multilon DN-1530B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 30 % filler. Improved stiffness and high fluidity realizes a thin wall..
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
19.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear
LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
19.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP DC0041PQ PC
LNP* THERMOCOMP* DC0041PQ is a compound based on Polycarbonate resin containing Carbon Fiber. Added feature of this grade is: Flame Retardant.
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
19.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp XF006S
LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region..
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
19.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA
LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized.
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X613 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller..
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X620/1 Novolac Phenolic
Glass fiber and graphite filled phenolic molding compound with excellent friction properties.USES: Low friction bearings, video recorder and compact disc parts. Not suitable for applications requir..
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X7010 Novolac Phenolic
Glass fiber reinforced molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
ISO 11359-1/-2
DSM Arnite® AV2 390 XT PET GF50
50% Glass Reinforced, Applications with extremely narrow tolerances
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® TW271B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® TW272B6 (PA46+PTFE)-CF30
30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
ISO 11359-1/-2
DSM Arnite® AV2 390 XL PET GF50
50% Glass Reinforced, Low outgassing
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 0.000 - 100 °C
19.4 µin/in-°F

@Temperature 32.0 - 212 °F
z direction; IPC TM-650 2.4.24
Arlon CLTE-P Pre-Preg Bonding Layer
Arlon's CLTE-P Prepreg Bonding Layer is a ceramic filled PTFE coated glass stock that is used as a bonding ply for CLTE, CLTE-X or CLTE-AT laminates. CLTE-P is a pre-preg material that consists of ..
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
z direction
Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic
High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED).
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 0.000 - 100 °C
19.4 µin/in-°F

@Temperature 32.0 - 212 °F
z direction; IPC TM-650 2.4.24
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite
Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a..
CTE, linear, Transverse to Flow 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X611 Novolac Phenolic
Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Complex precision parts with thin cross section and good mechanical properties e.g. in..
CTE, linear, Transverse to Flow 35.0 - 100 µm/m-°C
19.4 - 55.6 µin/in-°F
Average value: 68.7 µm/m-°C Grade Count:7
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
dry; ISO 11359-1/-2
DSM Stanyl® TC502 PA46
Thermal conductive material
CTE, linear, Transverse to Flow 35.0 - 116 µm/m-°C
19.4 - 64.4 µin/in-°F
Average value: 79.2 µm/m-°C Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..