Polymer Property : CTE, linear, Transverse to Flow = 32.9 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 59.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
32.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA
LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 59.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
32.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific)
LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated.