Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 18.0 - 27.0 µm/m-°C
10.0 - 15.0 µin/in-°F
Average value: 23.0 µm/m-°C Grade Count:4
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..