Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 177 µm/m-°C

@Temperature -30.0 - 30.0 °C
98.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp YF005
LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 177 µm/m-°C

@Temperature -30.0 - 30.0 °C
98.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP YF005 POLYESTER ELASTOMER
LNP* THERMOCOMP* YF005 is a compound based on Polyester Elastomer resin containing 25% Glass Fiber.
CTE, linear, Transverse to Flow 177 µm/m-°C

@Temperature 20.0 °C
98.3 µin/in-°F

@Temperature 68.0 °F
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer
ISO data as provided by the manufacturer, Eastman Chemical
CTE, linear, Transverse to Flow 177 µm/m-°C

@Temperature 20.0 °C
98.3 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® LT 6040IH Nylon (Conditioned)
ISO data provided by the manufacturer, Arkema.
CTE, linear, Transverse to Flow 177 µm/m-°C

@Temperature 0.000 - 100 °C
98.3 µin/in-°F

@Temperature 32.0 - 212 °F
z direction; IPC TM-650 2.4.24
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi..
CTE, linear, Transverse to Flow 177 µm/m-°C

@Temperature 20.0 °C
98.3 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® LT 6040ISH Nylon (Conditioned)
ISO data provided by the manufacturer, Arkema.
CTE, linear, Transverse to Flow 177 µm/m-°C

@Temperature 20.0 °C
98.3 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® LT 6040 Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good ..