Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 151 µm/m-°C @Temperature 20.0 °C |
83.9 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 130-33 Cellulose Acetate
(discontinued **) 33% Plasticized, contains 100% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Transverse to Flow | 151 µm/m-°C @Temperature 23.0 - 60.0 °C |
83.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY M3000 PP (Europe-Africa-Middle East) LNP* Stat-loy* M3000 is a compound based on Polypropylene resin. Added features of this material include: Antistat, High Impact. |