Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 145 µm/m-°C @Temperature 20.0 °C |
80.6 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 105-28 Cellulose Acetate
(discontinued **) 28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Transverse to Flow | 145 µm/m-°C @Temperature -30.0 - 30.0 °C |
80.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 145 µm/m-°C @Temperature 23.0 - 60.0 °C |
80.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp MK001AS PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MK001AS is a compound based on Polypropylene resin containing Mineral. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |