Polymer Property : CTE, linear, Transverse to Flow = 137 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 137 µm/m-°C

@Temperature 20.0 °C
76.1 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 383A-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Transverse to Flow 137 µm/m-°C

@Temperature 23.0 - 60.0 °C
76.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP WFI18 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WFI18 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Silicone.
CTE, linear, Transverse to Flow 137 µm/m-°C

@Temperature -30.0 - 30.0 °C
76.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6
LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat.
CTE, linear, Transverse to Flow 137 - 168 µm/m-°C
76.1 - 93.3 µin/in-°F
Average value: 148 µm/m-°C Grade Count:3
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
CTE, linear, Transverse to Flow 137 µm/m-°C

@Temperature 20.0 °C
76.1 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.