Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-PG6U (Dry) 33% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued **)& Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1,-2 |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66 PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 1100 000000 PBT PBT, non-reinforced, extrusion, injection molding, improved flowability |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 1700 000000 PBT PBT, non-reinforced, extrusion, food contact |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 3225 XF 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, improved flowability |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KU 2-7018 000000 PBT PBT, non-reinforced, extrusion, injection molding, impact modified |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® S 1517 000000 PBT PBT, non-reinforced, injection molding, extrusion, impact modified |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 3215 901510 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 60.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WAL34I PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WAL34I is a compound based on Polybutylene Terephalate resin containing PTFE, Aramid Fiber. Added features include Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 80.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East) XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature -20.0 - 150 °C |
72.2 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® SF-15 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20 LF grey PA12 Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has b.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LC-3H black PA12-CF30 Product description: Grilamid LC-3H BLACK is a Polyamide 12 injection molding product reinforced with 30 % carbon fibers. The product is inherently black and is only available in this color.Main Att.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 20.0 - 60.0 °C |
72.2 µin/in-°F @Temperature 68.0 - 140 °F |
TMS2 Perkin Elmer |
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBAFORM C 906 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont .. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® SF-10 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® TS 3220 901510 PBT + PET, 20% Glass Fiber PBT+PET, 20% glass fibers, injection molding, impact modified, low tendency to warp, improved surface finish |