Polymer Property : CTE, linear, Transverse to Flow = 120 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 84.0 - 120 µm/m-°C
46.7 - 66.7 µin/in-°F
Average value: 103 µm/m-°C Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
CTE, linear, Transverse to Flow 80.0 - 120 µm/m-°C
44.4 - 66.7 µin/in-°F
Average value: 96.0 µm/m-°C Grade Count:5
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
CTE, linear, Transverse to Flow 80.0 - 120 µm/m-°C
44.4 - 66.7 µin/in-°F
Average value: 98.8 µm/m-°C Grade Count:8
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
CTE, linear, Transverse to Flow 90.0 - 120 µm/m-°C
50.0 - 66.7 µin/in-°F
Average value: 107 µm/m-°C Grade Count:49
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
CTE, linear, Transverse to Flow 75.0 - 120 µm/m-°C
41.7 - 66.7 µin/in-°F
Average value: 97.0 µm/m-°C Grade Count:4
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
CTE, linear, Transverse to Flow 70.0 - 120 µm/m-°C
38.9 - 66.7 µin/in-°F
Average value: 97.2 µm/m-°C Grade Count:18
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
CTE, linear, Transverse to Flow 60.0 - 120 µm/m-°C

@Temperature 23.0 - 80.0 °C
33.3 - 66.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® C3U PA66/6 (Dry)
Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance.
CTE, linear, Transverse to Flow 80.0 - 120 µm/m-°C

@Temperature 23.0 - 55.0 °C
44.4 - 66.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
BASF Ultramid® Seal-Fit PA6/66 (Dry)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
CTE, linear, Transverse to Flow 40.0 - 120 µm/m-°C
22.2 - 66.7 µin/in-°F
Average value: 80.8 µm/m-°C Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..