Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 195 µm/m-°C @Temperature 23.0 - 60.0 °C |
108 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP YF003S Polyester Elastomer (Europe-Africa-Middle East) LNP* THERMOCOMP* YF003S is a compound based on Polyester Elastomer containing Glass Fiber. Added features include; Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 194 µm/m-°C @Temperature 0.000 - 100 °C |
108 µin/in-°F @Temperature 32.0 - 212 °F |
z direction; IPC TM-650 2.4.24 |
Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 233 uses a medium fiberglass/PTFE ratio to balance lower dielectric constant and improved dissipation factor without sacrificing mechanical properties.Cross Plied Woven Fiberglass, alternatin.. |