Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 106 µm/m-°C @Temperature -30.0 - 30.0 °C |
58.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 106 µm/m-°C @Temperature -30.0 - 30.0 °C |
58.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass. |