Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 0.700 µm/m-°C

@Temperature -30.0 - 30.0 °C
0.389 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6
LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am..
CTE, linear, Transverse to Flow 0.700 µm/m-°C

@Temperature -30.0 - 30.0 °C
0.389 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON DE003M PC
LNP* STAT-KON* DE003M is a compound based on Polycarbonate containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive.