Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 76.1 °C @Thickness 6.35 mm |
169 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.1 °C @Thickness 6.35 mm |
169 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.1 °C @Thickness 6.35 mm |
169 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.1 °C @Thickness 6.35 mm |
169 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.1 °C @Thickness 6.35 mm |
169 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.1 °C @Thickness 6.35 mm |
169 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not.. |