Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 74.0 °C @Thickness 3.20 mm |
165 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 74.0 °C @Thickness 3.20 mm |
165 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |