Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C

@Thickness 6.35 mm
219 °F

@Thickness 0.250 in
annealed, 120°C/hr; ASTM D648
Chi Mei Kibisan® PN137H SAN Resin, General Purpose
Information provided by Calsak Corporation
Deflection Temperature at 1.8 MPa (264 psi) 104 °C

@Thickness 3.18 mm
219 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC)
Geon LC500 CPVC is an extrusion grade rigid compound. It is designed for applications where enhanced resistance at elevated temperatures is needed. LC500 demonstrates ease of processing with excelle..