Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C

@Thickness 3.20 mm
203 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Cycolac® X17 ABS
Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C

@Thickness 6.40 mm
203 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications.
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C

@Thickness 6.40 mm
203 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific)
Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications.
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C

@Thickness 3.20 mm
203 °F

@Thickness 0.126 in
Annealed; ASTM-D648
Ineos ABS Lustran® 308 ABS, Medical Grade
Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi..
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C

@Thickness 6.35 mm
203 °F

@Thickness 0.250 in
unannealed, 120°C/hr; ASTM D648
Chi Mei Kibisan® PN137H SAN Resin, General Purpose
Information provided by Calsak Corporation