Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 4.00 mm
261 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1200-15 Polycarbonate Resin
Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 4.00 mm
261 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1201-15 Polycarbonate Resin
Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 4.00 mm
261 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1201-18 Polycarbonate Resin
Description: LUPOY PC 1201-18 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 4.00 mm
261 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1300-15 Polycarbonate Resin
Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 4.00 mm
261 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 3010-15 Polycarbonate Resin
Description: LUPOY PC 3010-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 4.00 mm
261 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 3030-15 Polycarbonate Resin
Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 4.00 mm
261 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 4.00 mm
261 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1303-15 Polycarbonate Resin
Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 4.00 mm
261 °F

@Thickness 0.157 in
Unannealed; ASTM D648
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin
Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 3.20 mm
261 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC
LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121.
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 6.40 mm
261 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC
LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121.
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 3.20 mm
261 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Asia Pacific)
Alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121.
Deflection Temperature at 1.8 MPa (264 psi) 127 °C

@Thickness 6.40 mm
261 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Asia Pacific)
Alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121.