Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Treatment Temp. 60.0 °C, Thickness 3.18 mm |
194 °F @Treatment Temp. 140 °F, Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy) VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 3.18 mm |
194 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426 Black 2880.Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 3.18 mm |
194 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 3.17 mm |
194 °F @Thickness 0.125 in |
Unannealed; ASTM-D648 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 3.20 mm |
194 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |