Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 88.0 °C @Thickness 3.20 mm |
190 °F @Thickness 0.126 in |
Unannealed; ASTM-D648 |
Ineos ABS Lustran® 308 ABS, Medical Grade Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.0 °C @Thickness 6.40 mm |
190 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.0 °C @Thickness 6.40 mm |
190 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical XG569C MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.0 °C @Thickness 3.20 mm |
190 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |