Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C @Thickness 6.35 mm |
165 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C @Thickness 6.35 mm |
165 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C @Thickness 6.35 mm |
165 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C @Thickness 6.35 mm |
165 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding MR900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C @Thickness 6.35 mm |
165 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |