Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 212 °C @Thickness 6.40 mm |
414 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM 2110EPR PEI 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 212 °C @Thickness 6.40 mm |
414 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific) 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 212 °C @Thickness 6.40 mm |
414 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM 2212EPR PEI 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 212 °C @Thickness 6.40 mm |
414 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific) 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 212 °C @Thickness 3.20 mm |
414 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 420SE0U PBT (Asia Pacific) UV-Stabilized version of 420SE0. |