Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 104 PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 3.20 mm |
279 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® FXE121R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). MFR 18.2. Internal mold release. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® FXE121R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). MFR 18.2. Internal mold release. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HPS6 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SFX123RU PC SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 3.20 mm |
279 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SFX123RU PC SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SFX123RU PC (Asia Pacific) SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 3.20 mm |
279 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SFX123RU PC (Asia Pacific) SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 137 °C @Thickness 6.40 mm |
279 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |