Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C

@Thickness 6.35 mm
172 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C

@Thickness 6.35 mm
172 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C

@Thickness 6.35 mm
172 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C

@Thickness 6.35 mm
172 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C

@Thickness 6.35 mm
172 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C

@Thickness 6.35 mm
172 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not..
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C

@Thickness 6.35 mm
172 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Geon™ HTX M6215 Polyvinyl Chloride Alloy (PVC Alloy)
It is recommended that the compound pellets be dried for 3 to 4 hours at 150 deg. F.Information provided by PolyOne