Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C @Thickness 3.20 mm |
268 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C @Thickness 3.20 mm |
268 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl N1251 PPE+PS ECO-FLO(tm). ECO conforming, non-halogen flame retardant PPE+PS. High flow. Electrical and Business Equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C @Thickness 3.20 mm |
268 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL NH5120 PPE+PS Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 131 °C @Thickness 3.20 mm |
268 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |