Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 385 °C | 725 °F | |
Hybrid Plastics Nanoreinforced® PM 1215 Polyimide The homogeneous dispersion of POSS® cages within polyimide provides enhanced control over chain dynamics which increases the toughness and damage tolerance over conventional polyimide. The chemic.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | |
Hybrid Plastics Nanoreinforced® POSS® 5% POSS-polyimide Nanoreinforced® POSS® Polyimide is a hybrid nanocomposite that can serve as oxidation resistant and highly bondable form of polyimide. Upon exposure to oxidizing oxygen the POSS® polyimide .. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | |
Hybrid Plastics Nanoreinforced® POSS® Polyimide Nanoreinforced® POSS® Polyimide is a hybrid nanocomposite that can serve as oxidation resistant and highly bondable form of polyimide. Upon exposure to oxidizing oxygen the POSS® polyimide .. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 100A Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 100EN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 100KN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 100VN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 100ZT Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 200A Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an ar.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 200EN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications requ.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 200FPC Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thickn.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 300A Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 300FPC Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 300KN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 300VN Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 300ZT Polyimide Film, 75 Micron Thickness Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 500A Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an .. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 500FPC Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thic.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 500VN Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available .. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 500ZT Polyimide Film, 125 Micron Thickness Film thickness 125 micron (5.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available .. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 50EN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 50FPC Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 50KN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 50VN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 50ZT Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 100FPC Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 200KN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianh.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 200ZT Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available in.. |
|||
Glass Transition Temp, Tg | 385 °C | 725 °F | Value for Kapton® HN |
DuPont™ Kapton® 200VN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available in.. |