Thermal Properties Metric English Comments
Glass Transition Temp, Tg 15.0 °C
59.0 °F
Humiseal 1B31 Acrylic Conformal Coating
Humiseal 1B31 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C ApprovedPasses thermal shock test (MI..
Glass Transition Temp, Tg 15.0 °C
59.0 °F
Humiseal 1B31LSE Acrylic Conformal Coating
Humiseal 1B31LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C Approval PendingPasses thermal sho..
Glass Transition Temp, Tg 15.0 °C
59.0 °F
ASTM E1356
SK Chemicals SKYTHANE® U1731C Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Glass Transition Temp, Tg 15.0 °C
59.0 °F
ASTM E1356
SK Chemicals SKYTHANE® UB220 Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Glass Transition Temp, Tg 15.0 °C
59.0 °F
ASTM E1356
SK Chemicals SKYTHANE® US106B Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Glass Transition Temp, Tg 15.0 °C
59.0 °F
Styron DL 216 NAD Carboxylated SB
Performance Features: High filler tolerance, formulation flexibilityApplications: General Purpose AdhesiveNorth AmericaInformation provided by Styron
Glass Transition Temp, Tg 15.0 °C
59.0 °F
10°C/min
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..
Glass Transition Temp, Tg 15.0 °C
59.0 °F
Mid-Point
3M Scotch-Weld™ DP-105 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s..
Glass Transition Temp, Tg 15.0 °C
59.0 °F
Mid-Point
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days ..
Glass Transition Temp, Tg 15.0 - 20.0 °C
59.0 - 68.0 °F
3M Novec™ FC-4432 Fluorosurfactant
3M fluorosurfactant FC-4432 is a non-ionic polymeric fluorochemical surfactant that offers excellent wetting, leveling and flow control in a variety of waterborne, solvent-borne and high-solids orga..