Thermal Properties Metric English Comments
Glass Transition Temp, Tg 13.0 °C
55.4 °F
DSC
Solvay Specialty Polymers Diofan® P 530 Polyvinylidene Chloride (PVDC)
Diofan® P 530 is a one-component, water-based dispersion of a polyvinylidene chloride (PVDC) copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances.This ma..
Glass Transition Temp, Tg 13.0 °C
55.4 °F
Film; DSC
Solvay Specialty Polymers Diofan® P530 Polyvinylidene Chloride (PVDC)  (discontinued **)
DIOFAN® P530 is an one-component latex, water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. Developed..
Glass Transition Temp, Tg 13.0 °C
55.4 °F
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M