Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 54.0 °C | 129 °F | TM R050-25 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Glass Transition Temp, Tg | 54.0 °C | 129 °F | Ultimate Tg |
Tra-Con Tra-Bond 2135D High Impact Epoxy Adhesive TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact stre.. |
|||
Glass Transition Temp, Tg | 54.0 °C | 129 °F | Ultimate Tg |
Tra-Con Tra-Bond FDA2 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and rec.. |
|||
Glass Transition Temp, Tg | 54.0 °C | 129 °F | Ultimate Tg |
Tra-Con Tra-Bond FDA2YL02 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-2 YL02 is a medium viscosity epoxy resin system specifically developed for adhesive and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug.. |
|||
Glass Transition Temp, Tg | 54.0 °C | 129 °F | Ultimate Tg |
Tra-Con Tra-Bond 216H01 Blush-Free Non-Sag Structural Epoxy Adhesive TRA-BOND 216H01 is a two-part epoxy adhesive specifically formulated to be non-sagging and have improved adhesion to smooth, non-porous substrates such as glass, ceramic, stainless steel, etc. This .. |
|||
Glass Transition Temp, Tg | 54.0 °C | 129 °F | |
Atom Adhesives AA-BOND FDA2 Epoxy Adhesive AA-BOND FDA2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and recei.. |
|||
Glass Transition Temp, Tg | 54.0 °C | 129 °F | |
3M Scotchcast™ 4 Electrical Insulating Resin 3M Scotchcast Electrical Insulating Resin 4 is a two-part, epoxy insulating and encapsulating resin. This resin, mixed in its unique two-part bag, generates its own heat to cure. Its compatibility w.. |
|||
Glass Transition Temp, Tg | 54.0 °C | 129 °F | |
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive AA-SUPERTHERM 195 is a two component, thermally conductive epoxy system recommended for staking transistors, diodes, resistors, integrated circuits and other heat sensitive components to printed cir.. |
|||
Glass Transition Temp, Tg | 54.0 - 60.0 °C | 129 - 140 °F | Average value: 56.0 °C Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Glass Transition Temp, Tg | 54.0 °C | 129 °F | TM R050-25 |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |