Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | >= 280 °C | >= 536 °F | Condition A; IPC-TM-650 2.4.24 |
Rogers Corporation RO4003C Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
Glass Transition Temp, Tg | >= 280 °C | >= 536 °F | Condition A; IPC-TM-650 2.4.24 |
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
Glass Transition Temp, Tg | >= 280 °C @Temperature -60.0 - 300 °C |
>= 536 °F @Temperature -76.0 - 572 °F |
10°C/min, TGA; IPC-TM-650 2.4.24 |
Rogers Corporation RO4450B Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Glass Transition Temp, Tg | >= 280 °C | >= 536 °F | TGA, Condition A; IPC-TM-650 2.4.24 |
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
Glass Transition Temp, Tg | >= 280 °C | >= 536 °F | TGA, Condition A; IPC-TM-650 2.4.24 |
Rogers Corporation RO4534 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
Glass Transition Temp, Tg | >= 280 °C | >= 536 °F | TGA, Condition A; IPC-TM-650 2.4.24 |
Rogers Corporation RO4535 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
Glass Transition Temp, Tg | >= 280 °C | >= 536 °F | TGA, Condition A; IPC-TM-650 2.4.24 |
Rogers Corporation RO4835 Hydrocarbon Ceramic Laminate, Improved Oxidation Resistance Features and Benefits:Significantly improved oxidation resistance compared to typical thermoset microwave materialsDesigned for performance sensitive, high volume applicationsLow loss - Excellent el.. |
|||
Glass Transition Temp, Tg | 280 °C | 536 °F | DSC, 20°C/min.; ISO 11357-1/-2 |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Glass Transition Temp, Tg | 280 °C | 536 °F | DSC, 20°C/min.; ISO 11357-1/-2 |
Quadrant EPP Duratron® PAI T4301 PAI + graphite + PTFE, extruded (ISO Data) The addition of PTFE and graphite provides higher wear resistance and lower coefficient of friction compared to the unfilled grade as well as a lower tendency to stick-slip. Duratron T4301 PAI also .. |
|||
Glass Transition Temp, Tg | 280 °C | 536 °F | DSC, 20°C/min.; ISO 11357-1/-2 |
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data) Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Glass Transition Temp, Tg | 280 °C | 536 °F | DSC, 20°C/min.; ISO 11357-1/-2 |
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data) Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo.. |
|||
Glass Transition Temp, Tg | >= 280 °C | >= 536 °F | TMA; ASTM D3850 |
Rogers Corporation LoPro™ RO4730 Antenna Grade Non-PTFE Laminate RO4730 LoPro Antenna Grade Laminates are fully compatible with conventional FR-4 and high temperature lead-free solder processing. The resin systems of RO4730 dielectric materials are designed to p.. |
|||
Glass Transition Temp, Tg | >= 280 °C @Temperature -60.0 - 300 °C |
>= 536 °F @Temperature -76.0 - 572 °F |
10°C/min, TGA; IPC-TM-650 2.4.24 |
Rogers Corporation RO4450F Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Glass Transition Temp, Tg | 280 °C | 536 °F | DSC, 20°C/min.; ISO 11357-1/-2 |
Quadrant EPP Duratron® PAI T4503 PAI, unfilled, compression moulded (ISO Data) Compression moulded Duratron T4503 PAI is similar in composition to Duratron T4203 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Glass Transition Temp, Tg | 280 °C | 536 °F | |
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance .. |
|||
Glass Transition Temp, Tg | 280 °C | 536 °F | DSC, 20°C/min.; ISO 11357-1/-2 |
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data) This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s.. |