Thermal Properties Metric English Comments
Glass Transition Temp, Tg 49.0 °C
120 °F
Dynamic Viscoelasticity
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
48 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, specialty applications. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now p..
Glass Transition Temp, Tg 49.0 °C
120 °F
Ultimate Tg
Tra-Con Tra-Duct 2960 Snap Cure Electrically Conductive Silver-Filled Epoxy
TRA-DUCT 2960 is a one or two-part, specially refined and processed silver filled adhesive for high speed manufacturing. Recommended for the microelectronic, automotive computer and telecommunicatio..
Glass Transition Temp, Tg 49.0 °C
120 °F
Mid-point
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Glass Transition Temp, Tg 49.0 °C
120 °F
Mid-point
3M Scotch-Weld™ DP270 Clear Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Glass Transition Temp, Tg 49.0 °C
120 °F
Ultimate Tg; TMA
Tra-Con Tra-Bond 516H01 Low Viscosity Room Temperature Cure Adhesive
TRA-BOND 516H01 is a room temperature curing, low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors, including Pre-Mixed and Frozen applications. It has also been use..
Glass Transition Temp, Tg 49.0 °C
120 °F
ASTM E1545-00
DSM Somos® ProtoCast™ AF 19122 Antimony-free Liquid Photopolymer
Product DescriptionDSM Somos® ProtoCast™ AF 19122 is an antimony-free liquid photopolymer specifically formulated for producing investment casting patterns.ApplicationsIdeal for use in foundry app..
Copyright © lookpolymers.com All Rights Reserved