Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -5.00 - 155 °C | 23.0 - 311 °F | Average value: 74.0 °C Grade Count:80 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Glass Transition Temp, Tg | 145 - 155 °C | 293 - 311 °F | DMA |
Hexcel® HexPly® 1458 160°C-180°C Curing Epoxy Matrix HexPly® 1458 is a self-extinguishing and self-adhesive modified epoxy resin system for monolithic and sandwich structures. HexPly® 1458 has excellent temperature and moisture resistance. It has a .. |