Thermal Properties Metric English Comments
Glass Transition Temp, Tg 118 °C
244 °F
ASTM D4065
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC
AMC™ 8590 BK is a vinyl ester, chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant,..
Glass Transition Temp, Tg 118 °C
244 °F
DMA
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC
AMC™ 8592 is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat ..
Glass Transition Temp, Tg 118 °C
244 °F
ASTM D4065
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC
AMC™ 8593 NT is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high he..
Glass Transition Temp, Tg 118 °C
244 °F
TM R050-25
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy
EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi..
Glass Transition Temp, Tg 118 °C
244 °F
Silicone Property; ASTM D3418
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu..
Glass Transition Temp, Tg 118 °C
244 °F
Armstrong A-40 Epoxy Adhesive
Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re..
Glass Transition Temp, Tg 118 - 200 °C
244 - 392 °F
Average value: 169 °C Grade Count:7
Overview of materials for Vinyl Ester Sheet Molding Compound