Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 116 °C | 241 °F | DAM (SSYS) |
Proto3000 ABSi Fused Deposition Modeling Polymer Description: Stratasys ABSi is an ideal material for conceptual modeling, functional prototyping and direct digital manufacturing. Its strength is superior to standard Stratasys ABS, and the translu.. |
|||
Glass Transition Temp, Tg | 116 °C | 241 °F | dry |
Henkel Hysol EA 9628H Film Adhesive First generation, modified epoxy film, high peel strength, good stress, environmental resistance and structural propertiesApplications: Composite Bonding, Metal & Honeycomb BondingData from .060 psf.. |
|||
Glass Transition Temp, Tg | 116 °C | 241 °F | DSC (SSYS) |
Stratasys® ABSi Stratasys is the only company that gives engineers the ability to manufacture real ABSi industrial thermoplastic parts direct from digital files. ABSi parts can be used from conceptual prototyping t.. |
|||
Glass Transition Temp, Tg | 116 °C | 241 °F | Ultimate Tg |
Tra-Con Tra-Bond F253 Color Keyed High Temperature Epoxy Adhesive TRA-BOND F253 is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status. The unmixed components are light yellow; the mixt.. |
|||
Glass Transition Temp, Tg | 116 °C | 241 °F | Dry |
Hexcel® HexPly® M10E Epoxy Resin HexPly® M10E is an epoxy resin system preimpregnated into aramid, glass or graphite multiaxial fabrics and unidirectional fibers. M10E prepregs are recommended for the production of low cost, large.. |
|||
Glass Transition Temp, Tg | 116 °C | 241 °F | Wet |
Hexcel® HexPly® 8551-7 Epoxy Matrix HexPly® 8551-7 is an amine-cured, toughened epoxy resin system supplied with unidirectional graphite fibers. Typical reinforcement is continuous IM7 (intermediate modulus) graphite filaments. HexPl.. |
|||
Glass Transition Temp, Tg | 116 °C | 241 °F | |
Atom Adhesives AA-BOND F253 Epoxy Adhesive AA-BOND F253 is a low viscosity, high temperature, two-part epoxy formulation that changes color during the curing process to indicate cure status.Appearance: Unmixed-Light Yellow; Mixed – Greenish.. |