Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 83.0 - 100 °C | 181 - 212 °F | Average value: 90.5 °C Grade Count:6 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Glass Transition Temp, Tg | 81.0 - 100 °C | 178 - 212 °F | ASTM D3418 |
BiologiQ EcoStarch GS270 Thermoplastic Starch BiologiQ GS270 is a plasticized thermoplastic starch (TPS) called EcoStarch Resin (ESR). It is suitable for blending with petrochemical or bioresins where biobased content is desired. It Can be us.. |