Thermal Properties Metric English Comments
Glass Transition Temp, Tg 87.0 °C
189 °F
ASTM D1525
Eastman Eastar 5445 PCTG Copolyester, Injection Molded  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..
Glass Transition Temp, Tg 87.0 °C
189 °F
ASTM D1525
Eastman Eastar 5445 PCTG Copolyester, Film  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..
Glass Transition Temp, Tg 87.0 °C
189 °F
DSC
Kolon NOPLA® KE131 PEN-PET Copolyester
NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac..
Glass Transition Temp, Tg 87.0 °C
189 °F
Solvay SIPOMER® WAM II Composition Based On Methacrylamidoethyl Ethylene Urea
Description: Specialty monomer for Wet Adhesion PromotionIdentification: COMPOSITION BASED ON METHACRYLAMIDOETHYL ETHYLENE UREACAS: 3089 – 19 – 8Solubility: Total in water Polymer Test (10..
Glass Transition Temp, Tg 87.0 °C
189 °F
Ultimate Tg
Tra-Con Tra-Bond 716K01 Radio Opaque Epoxy Adhesive
TRA-BOND 716K01 is a low viscosity epoxy resin system specifically developed for adhesive coating applications where radio opacity is required. This two part dark grey adhesive is commonly used for ..
Glass Transition Temp, Tg 87.0 °C
189 °F
Onset, Cure Temperature: 140°C, Cure Time: 10 min
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy
HexPly® M52 is a modified epoxy matrix with good mechanical and temperature performance, specifically designed for rapid press curing. HexPly® M52 is ideal for small to high volume industrial appl..
Glass Transition Temp, Tg 87.0 °C
189 °F
Loctite® Durabond® E-20NS Epoxy Adhesive
Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli..
Glass Transition Temp, Tg 87.0 °C
189 °F
Armstrong A-3/A Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..