Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 182 °C | 360 °F | ASTM D4065-01 |
Premix Premi-Glas® 1261-28 VE Glass Reinforced Vinyl Ester TMC Description: Premi-Glas® 1261-28 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Excellent thermal stability an.. |
|||
Glass Transition Temp, Tg | 182 °C | 360 °F | dry |
Henkel Hysol EA 9657 Film Adhesive High temperature, service film adhesive designed for high honeycomb peel in a reticulated sound suppression structure. Qualified to BMS 5-137. Data from .080 psf, 400 g / m2.Applications: Composite .. |