Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 15.0 °C | 59.0 °F | |
Humiseal 1B31 Acrylic Conformal Coating Humiseal 1B31 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C ApprovedPasses thermal shock test (MI.. |
|||
Glass Transition Temp, Tg | 15.0 °C | 59.0 °F | |
Humiseal 1B31LSE Acrylic Conformal Coating Humiseal 1B31LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C Approval PendingPasses thermal sho.. |
|||
Glass Transition Temp, Tg | 15.0 °C | 59.0 °F | ASTM E1356 |
SK Chemicals SKYTHANE® U1731C Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Glass Transition Temp, Tg | 15.0 °C | 59.0 °F | ASTM E1356 |
SK Chemicals SKYTHANE® UB220 Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Glass Transition Temp, Tg | 15.0 °C | 59.0 °F | ASTM E1356 |
SK Chemicals SKYTHANE® US106B Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Glass Transition Temp, Tg | 15.0 °C | 59.0 °F | |
Styron DL 216 NAD Carboxylated SB Performance Features: High filler tolerance, formulation flexibilityApplications: General Purpose AdhesiveNorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | 15.0 °C | 59.0 °F | 10°C/min |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Glass Transition Temp, Tg | 15.0 °C | 59.0 °F | Mid-Point |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |
|||
Glass Transition Temp, Tg | 15.0 °C | 59.0 °F | Mid-Point |
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days .. |
|||
Glass Transition Temp, Tg | 15.0 - 20.0 °C | 59.0 - 68.0 °F | |
3M Novec™ FC-4432 Fluorosurfactant 3M fluorosurfactant FC-4432 is a non-ionic polymeric fluorochemical surfactant that offers excellent wetting, leveling and flow control in a variety of waterborne, solvent-borne and high-solids orga.. |