Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 134 °C | 273 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2300 Unsaturated Polyester UP BMC 2300 is a special BMC with exceptional high fire retardancy. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Fire retardanc.. |
|||
Glass Transition Temp, Tg | 134 °C | 273 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013F-04 is a high temperature film extrusion grade for blends. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity .. |
|||
Glass Transition Temp, Tg | 134 °C | 273 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Glass Transition Temp, Tg | 134 °C | 273 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high .. |