Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 13.0 °C | 55.4 °F | DSC |
Solvay Specialty Polymers Diofan® P 530 Polyvinylidene Chloride (PVDC) Diofan® P 530 is a one-component, water-based dispersion of a polyvinylidene chloride (PVDC) copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances.This ma.. |
|||
Glass Transition Temp, Tg | 13.0 °C | 55.4 °F | Film; DSC |
Solvay Specialty Polymers Diofan® P530 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® P530 is an one-component latex, water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. Developed.. |
|||
Glass Transition Temp, Tg | 13.0 °C | 55.4 °F | |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |