Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 51.0 °C | 124 °F | ASTM D3418 |
Eastman Eastobond 19411 Copolyester, Film Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so.. |
|||
Glass Transition Temp, Tg | 51.0 °C | 124 °F | ASTM D3418 |
Eastman Eastobond 19412 Copolyester, Film Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob.. |