Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Mallard Creek Polymers BarrierPro® 4555 Styrene-Butadiene Emulsion Barrier Pro® 4555 is a general purpose latex binder of low stiffness. It dries to form a soft but tough film. Its softness makes it excellent for damp proofing where films must remain flexible at.. |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Mallard Creek Polymers Rovene® 4560 Styrene-Butadiene Emulsion Description: ROVENE® 4560 is an anionic carboxylated styrene-butadiene copolymer latex designed for fast film formation and excellent water resistance. Features: Highly stableCured films are toug.. |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Mallard Creek Polymers ROVENE® 6020 SBR Latex Applications: Rovene® 6020 is a soft, carboxylated stryene-acrylic copolymer emulsion. The typical films are soft and strong with good water resistance and exhibit good resistance to discoloratio.. |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Mallard Creek Polymers Rovene® 6021 Styrene-Acrylic Emulsion Applications: Rovene® 6021 is a soft, carboxylated styrene-acrylic copolymer emulsion. The typical films are soft and strong with good water resistance and exhibit good resistance to discoloratio.. |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | DSC heating rate = -10° C/min |
Kuraray SEPTON® H5125 Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | Compound |
KKPC KOSYN SOL 5990 Solution Styrene Butadiene Rubber (S-SBR) Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It .. |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Styron XZ 94462.01 Carboxylated SB Performance Features: Good compatibility with natural rubber, flexibilityApplications: Leather BindingEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Styron XZ 94462.01 Carboxylated SB Performance Features: Good compatibility with natural rubber, flexibilityApplications: Leather BindingAsia PacificInformation provided by Styron |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Styron XZ 94462.01 Carboxylated SB Performance Features: Good compatibility with natural rubber, flexibilityApplications: Leather BindingLatin America/South AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Styron XZ 94463.01 Functionalized SB Performance Features: High film elongation, good bonding adhesion to paper, film and aluminum, heat sealable, low odor, high water resistanceApplications: General Purpose Adhesive and Heat SealableE.. |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Styron DL 447 SB Latex Performance Features: Integrated antifoam, low e-modulus mortars, freeze/thaw stabilityApplications: 2K Cementious and Modified ConcreteAsia PacificInformation provided by Styron |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Styron XZ 94447.00 SB Latex Performance Features: Integrated antifoam, low e-modulus mortars, freeze/thaw stabilityApplications: 2K Cementious, Grouts and Modified ConcreteEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | |
Styron XZ 94462.01 Carboxylated SB Performance Features: Soft low tack film, high elongationApplications: Fiber Binding and NonwovensEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | DSC |
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Glass Transition Temp, Tg | -17.0 °C | 1.40 °F | DSC, modulated, midpoint |
DuPont Performance Polymers VTR 8650 (GBL-S) Peroxide Cured Fluoroelastomer (FKM) Formulation FormulationVTR 8650 |