Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glass Transition Temp, Tg = 1.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 1.00 °C
33.8 °F
Mallard Creek Polymers BarrierPro® 4550 SBR Emulsion
BARRIER PRO® 4550 is an anionic carboxylated styrene-butadiene copolymer latex containing a non-staining antioxidant. Features: highly stable, good compatibility with fillers and pigments, etc., ..
Glass Transition Temp, Tg 1.00 °C
33.8 °F
Styron DL 499 SB Latex
Performance Features: APEO free, excellent adhesion and alkaline stability, Integrated antifoamApplications: 2K Cementious, Grouts and Modified ConcreteAsia PacificInformation provided by Styron
Glass Transition Temp, Tg 1.00 °C
33.8 °F
Styron XU 31586.00 Carboxylated SB
Performance Features: Good MVTR, good adhesion to sheathing substratesApplications: EIFS, ETICSNorth AmericaInformation provided by Styron
Glass Transition Temp, Tg 1.00 °C
33.8 °F
Styron XZ 97222.00 SB Latex
Performance Features: APEO free, excellent adhesion and alkaline stabilityApplications: 2K Cementious, EIFS, ETICS, Grouts and Modified ConcreteEuropeInformation provided by Styron
Glass Transition Temp, Tg 1.00 °C
33.8 °F
Styron DL499 SB Latex
Performance Features: APEO free, excellent adhesion and alkaline stability, integrated antifoamApplications: 2K Cementious, EIFS, ETICS, Grouts and Modified ConcreteEuropeInformation provided by Sty..
Glass Transition Temp, Tg 1.00 °C
33.8 °F
Unitika elitel UE3223 Polyester, Flake
Adhesive agent, Resin modifier, Good solubility, Low temperature sealingUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from pro..
Glass Transition Temp, Tg 1.00 °C
33.8 °F
Styron XQ 83271.00 Modified SB
Performance Features: Control of moisture vapor permeability, APEO-freeApplications: Waterproofing Membranes and Modified ConcreteAsia PacificInformation provided by Styron
Copyright © lookpolymers.com All Rights Reserved