Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -58.0 °C | -72.4 °F | Dow Method |
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP) AFFINITY™ GA 1900 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and.. |
|||
Glass Transition Temp, Tg | -58.0 °C | -72.4 °F | DSC, 10°C/min (inf); DuPont Test |
Dow Engage® ENX 7458.00 Ethylene-Butene Copolymer Description: ENX 7458.00 is a unique broader molecular weight distribution ethylene-butene copolymer that offers excellent flow and impact properties and is ideally suited for plastics modification... |
|||
Glass Transition Temp, Tg | -58.0 °C | -72.4 °F | DMA @ 10 Hz; ASTM D2240 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2590 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |