Polymer Property : Glass Transition Temp, Tg = -54.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -47.8 °C
-54.0 °F
DSC, 18ºF/min; DIN 51.007
Lubrizol Advanced Materials PEARLTHANE® 16N85UV Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 16N85UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless, combining hardness with excellent mechanical properties and excellent hydro..
Glass Transition Temp, Tg -47.8 °C
-54.0 °F
Dow Method
Dow FLEXOMER™ GERS-1088 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ GERS-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to..
Glass Transition Temp, Tg -47.8 °C
-54.0 °F
DSC, 50°F/min; DIN 51.007
Lubrizol Advanced Materials Pearlthane® ECO D20N88 Thermoplastic Polyurethane  (discontinued **)
PEARLTHANE® ECO D20N88 is a 86 Shore A, High Performance natural TPU based on Renewable Sources with ca. 60% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicatio..