Polymer Property : Glass Transition Temp, Tg = -45.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
10°C/min; ISO 11357-1/-2
DuPont Performance Polymers Hytrel® HTR237BG BK320 TPC-ET  (Unverified Data**)
Hytrel® HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal durometer hardness of 45D, is pigmented black with fine particle size carbon black an..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Mallard Creek Polymers ROVENE® 6050 Acrylic Emulsion
ROVENE® 6050 is a very soft acrylic latex emulsion specifically designed for formulation of permanent label adhesives. Its relative high molecular weight allows the formulation of permanent label..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Mallard Creek Polymers Rovene® 6104 Resin Supported Emulsion
Rovene® 6104 is a very soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6104 can be used as the film fo..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Mallard Creek Polymers ROVENE® 97982 Acrylic Emulsion
ROVENE® 97982 is a very soft acrylic latex emulsion suggested as a base resin in flexible packaging laminating adhesives. Rovene® 97982 provides formulations with excellent clarity and UV stab..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
LG Chemical LC180 Polyolefin Elastomer
Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear application.Application: Polymer modification, Shoe sole, Film coe..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
DSC, 50°F/min; DIN 51.007
Lubrizol Advanced Materials Pearlthane® Maxi 12T85E Thermoplastic Polyurethane Elastomer
PEARLTHANE® MAXI 12T85E is a polyester based TPU, supplied in form of transparent, colorless pellets, featuring medium hardness, good mechanical properties and outstanding abrasion resistance. Th..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
ASTM E1356
SK Chemicals SKYTHANE® U0251M Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
ASTM E1356
SK Chemicals SKYTHANE® U101 Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Styron XZ 94462.04 Carboxylated SB
Performance Features: Very soft tacky filmApplications: Fiber Binding and NonwovensEuropeInformation provided by Styron
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Wanhua Chemical Wanthane® WHT-8180 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Wanhua Chemical Wanthane® WHT-8185 Polyether-Based TPU
Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Wanhua Chemical Wanthane® WHT-A885 Aliphatic TPU
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
DSC
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane
Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection ..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane
Features: Highly Elastic Compound and Good Recovery for a Rubber-Like CharacterUses: Flat Die/Film Extrusion and Blown Film and Injection Molding and Profile ExtrusionAvailable in Americas, Europe, ..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
DSC
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
ExxonMobil Method
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin
Product Description: Exact 9371 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
DSC, 10°C/min (inf); DuPont Test
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer
Description: ENR 7256.00 is a unique broader molecular weight distribution ethylene-butene copolymer with higher branching levels that offers excellent clarity, processing and performance in foams a..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
DSC, 10°C/min (inf); DuPont Test
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer
Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th..
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
DSC
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti..