Thermal Properties Metric English Comments
Glass Transition Temp, Tg -42.0 - -39.0 °C
-43.6 - -38.2 °F
(DMA) @ 1 Hz
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Glass Transition Temp, Tg -42.0 - -39.0 °C
-43.6 - -38.2 °F
(DMA) @ 1 Hz
Arkema Group Kynar Flex® 3120 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Glass Transition Temp, Tg -41.0 - -39.0 °C

@Frequency 1.00 Hz
-41.8 - -38.2 °F

@Frequency 1.00 Hz
DMA
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..