Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | Midpoint; ASTM E 1269 |
Huntsman IROGRAN® CA 117-200 DP TPU-Polyester Polyester-based TPUs that are specially designed for adhesives applications where high green strength and a fast crystallization rate are essential qualities.Information provided by Alliance Polymer.. |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | |
Huntsman KRYSTALFLEX® PE 192 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | |
Mallard Creek Polymers ROVENE® 4848 SBR Emulsion ROVENE® 4848 is a new developmental polymer specifically designed to be used in two part spray adhesives for open or closed cell foams and other contact and cold seal applications. Fast breaking .. |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | |
Mallard Creek Polymers ROVENE® 6005 Acrylic Emulsion ROVENE® 6005 is a very soft acrylic, high molecular weight latex emulsion specifically designed for formulation of permanent label adhesives. Its high molecular weight allows the formulation of p.. |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | DSC |
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos.. |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | |
Zeon Chemicals Hydrin® T3102 Polyepichlorohydrin Elastomer Hydrin T3102 is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with high oil fuel and solvent resistance. Compounds using Hydrin T3102 typically exhibit excellent low and high tem.. |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | |
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | DSC |
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin .. |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | Pellet sample |
BASF Elastollan® C85A10 (917) Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | DSC |
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E.. |
|||
Glass Transition Temp, Tg | -38.0 °C | -36.4 °F | Typical of rubber with 18% ACN content |
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber) Nitrile Rubbers are copolymers of butadiene and acrylonitrile. The term has also been applied to copolymers of other dienes and/or nitriles. Acrylonitrile content may range from 18-50%. Increasin.. |